Legering | Standard Strand Construction, MM | Modstand, ω/m | Nominel strengdiameter, MM | Måler pr. Kilo |
NICR 80/20 | 19 × 0,544 | 0,233-0.269 | 26 | |
NICR 80/20 | 19 × 0,61 | 0,205-0.250 | ||
NICR 80/20 | 19 × 0,523 | 0.276-0.306 | 2.67 | 30 |
NICR 80/20 | 19 × 0,574 | 2.87 | 25 | |
NICR 80/20 | 37 × 0,385 | 0.248-0.302 | 2,76 | 26 |
NICR 60/15 | 19 × 0,508 | 0.286-0.318 | ||
NICR 60/15 | 19 × 0,523 | 0.276-0.304 | 30 | |
Ni | 19 × 0,574 | 0,020-0,027 | 2.87 | 21 |
Detaljer
Egenskaber/klasse | CR20NI80 | CR30NI70 | CR15NI60 | CR20NI35 | CR20NI30 | |
Hovedkemisk sammensætning | Ni | Hvile | Hvile | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
Fe | ≤ 1,0 | ≤ 1,0 | Hvile | Hvile | Hvile | |
Maks. Kontinuerlig servicetemp. af element | 1200 | 1250 | 1150 | 1100 | 1100 | |
Resistivitet ved 20oC (μ ω · m) | 1.09 | 1.18 | 1.12 | 1,04 | 1,04 | |
Densitet (g/cm3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
Termisk ledningsevne (KJ/M · H · OC) | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
Koefficient for linjerudvidelse (α × 10-6/OC) | 18 | 17 | 17 | 19 | 19 | |
Smeltepunkt (ca.) (OC) | 1400 | 1380 | 1390 | 1390 | 1390 | |
Forlængelse ved brud (%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
Mikrografisk struktur | Austenite | Austenite | Austenite | Austenite | Austenite | |
Magnetiske egenskaber | ikke -magnetisk | ikke -magnetisk | ikke -magnetisk | ikke -magnetisk | ikke -magnetisk |
Kemisk sammensætning | Nikkel, krom |
Tilstand | Lys/syre hvid/oxideret farve |
Grad | Ni80Cr20, Ni70/30, Ni60Cr15, Ni60Cr23, Ni35Cr20Fe, Ni30Cr20 Ni80, Ni70, Ni60, Ni40, |
Fordel | Nichromes metallurgiske struktur giver dem en meget god plasticitet, når de er koldt. |
Egenskaber | Stabil ydeevne; Anti-oxidation; Korrosionsmodstand; Stabilitet i høj temperatur; Fremragende spiraldannende evne; Ensartet og smuk overfladetilstand uden pletter. |