Legeringstype / Ydeevne | 1Cr13Al4 | 0Cr25Al5 | 0Cr21Al6 | 0Cr23Al5 | 0Cr21Al4 | 0Cr21Al6Nb | 0Cr27Al7Mo2 | |
Komposition | Cr | 12,0-15,0 | 23,0-26,0 | 19,0-22,0 | 20,5-23,5 | 18,0-21,0 | 21,0-23,0 | 26,5-27,8 |
Al | 4,0-6,0 | 4,5-6,5 | 5,0-7,0 | 4.2-5.3 | 3,0-4,2 | 5,0-7,0 | 6,0-7,0 | |
Re | Belejligt | |||||||
Fe | Hvile | |||||||
Nb0,5 | Måned 1,8-2,2 | |||||||
Maks. kontinuerlig driftstemperatur for element (℃) | 950 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 | |
Modstand ved 20 ℃ (μm.m) | 1,25 | 1,42 | 1,42 | 1,35 | 1.23 | 1,45 | 1,53 | |
Densitet (g/cm3) | 7.4 | 7.1 | 7.16 | 7,25 | 7,35 | 7.1 | 7.1 | |
Termisk ledningsevne (kJ/mh℃) | 52,7 | 46,1 | 63,2 | 60,2 | 46,9 | 46,1 | – | |
Koefficient for linjeudvidelse (ax10-6/℃) | 15.4 | 16 | 14,7 | 15 | 13,5 | 16 | 16 | |
Smeltepunkt ca. (℃) | 1450 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 | |
Hårdhed (HB) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | |
Forlængelse ved brud (%) | >16 | >12 | >12 | >12 | >12 | >12 | >10 | |
Gentag bøjningsfrekvens (F/R) | >5 | >5 | >5 | >5 | >5 | >5 | >5 | |
Kontinuerlig servicetid (timer/℃) | – | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥80/1350 | ≥80/1350 | |
Trækstyrke (N/mm2) | 580-680 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 650-800 | |
Variation af areal (%) | 65-75 | 60-75 | 60-75 | 60-75 | 60-75 | 60-75 | 60-75 | |
Mikrografisk struktur | Ferrit | Ferrit | Ferrit | Ferrit | Ferrit | Ferrit | Ferrit | |
Magnetiske egenskaber | Magnetisk | Magnetisk | Magnetisk | Magnetisk | Magnetisk | Magnetisk | Magnetisk |
150 0000 2421